โ† All CWI Flashcard Decks

Practical Visual Inspection Flashcards

7 cards from real CWI practice questions. Tap to flip, then mark Knew It or Still Learning โ€” missed cards come back until you master them.

Read the first 7 Practical Visual Inspection flashcards as text
  1. During a visual inspection of a fillet weld, you observe that the weld face is excessively convex. What is the primary concern with this condition?

    Answer: It creates stress concentration at the weld toes

    Excessive convexity creates stress concentration at the weld toes, which can lead to fatigue cracking under cyclic loading.

  2. A CWI is inspecting a butt weld and notes the weld crown is lower than the base metal surface. This condition is known as:

    Answer: Underfill

    Underfill (also called insufficient fill) occurs when the weld face is below the surrounding base metal surface, reducing the weld cross-section.

  3. When visually inspecting for overlap on a fillet weld, you are looking for:

    Answer: Weld metal that has flowed beyond the fusion zone onto the base metal without fusing

    Overlap is unfused weld metal that extends beyond the weld toe onto the base metal, creating a notch-like condition.

  4. Which tool is most appropriate for measuring the depth of undercut in a weld?

    Answer: Undercut gauge or dial depth gauge

    An undercut gauge or dial depth gauge is specifically designed to measure the depth of groove undercut relative to the base metal surface.

  5. During visual inspection, you find surface porosity on a completed weld bead. Which of the following is the most likely cause?

    Answer: Contamination such as moisture, oil, or rust on the base metal or filler

    Surface porosity is most commonly caused by contamination (moisture, oil, rust, or mill scale) that releases gas during welding.

  6. A weld inspector measures a fillet weld leg size and finds it is 3/8 inch on one leg and 1/2 inch on the other. What condition does this describe?

    Answer: An unequal leg fillet weld

    When the two legs of a fillet weld differ in size, it is called an unequal leg fillet weld, which may or may not be acceptable depending on the drawing specification.

  7. What is the correct sequence for performing a visual inspection of a weld?

    Answer: Inspect before, during, and after welding

    AWS standards require visual inspection before (joint prep, fit-up), during (interpass), and after welding (final visual) for comprehensive quality assurance.